In cooling through this zone, ferrite is precipitated on the austenite grain boundaries. As the temperature is reduced, the austenite composition moves towards the eutectoid value, and at 727 C has ...
While it cools through this zone Fe 3 C is deposited on the austenite grain boundaries and the austenite composition moves to the eutectoid value. When the alloy reaches the eutectoid temperature the ...